Yadda za a warware da kuma hana lahani na simintin gyaran kafa?

Fitar da baƙin ƙarfe galibi yana haifar da lahani iri-iri a cikin aikin samarwa. Yanzu Shijiazhuang donghuan malleable baƙin ƙarfe fasaha co., Ltd gaya muku yadda za a hana irin wannan lahani ya kasance matsala da cewa simintin gyaran kafa masana'antun damu game da.

Taron samarwa ya fi amfani da tsarin simintin yashi na gargajiya don samar da simintin ƙarfe. A cikin samar da dogon lokaci, an gano cewa lahani na simintin da ke biyo baya sun fi faruwa a cikin simintin ƙarfe, kamar ramukan yashi, yashi mai mannewa, ramuka, ramuka, haɗa yashi da tabo, kumburi, yashi waɗannan.

1. Matakan rigakafin cutar trachoma:

(1) Tsananin sarrafa aikin gyare-gyaren yashi;

(2) Kafin rufe akwatin, warware yashin da ke iyo a saman madaidaicin gyare-gyare da kuma yashin yashi da kyau kuma a rufe akwatin a tsaye;

(3) Kafa tsarin software mai dacewa da inganci;

(4) saman saman kofin ya kamata ya zama santsi da tsabta, kuma ba za a iya samun yashi mai iyo ba.

2. Matakan kariya don yin yashi

(1) Yi amfani da yashi tare da babban juriya na wuta;

(2) Rage yawan zafin da ake zubawa a matsakaici da kuma ƙara yawan zubar da ruwa;

(3) Ƙaƙƙarfan ƙwayar yashi ya kamata ya zama babba (gaba ɗaya fiye da 85) kuma yana da kyau;

(4) Zaɓi riguna na gine-gine waɗanda ba sa fashe a yanayin zafi mai yawa kuma kada su shiga cikin narkakken ramuka.

Barka da zuwa tuntubar kamfaninmu don matsalolin simintin gyare-gyare daban-daban.